Zinc particles, zinc scars and rough patches on galvanized or Galvalume surfaces are among the most troublesome quality issues for steel mills. Many first suspect the zinc bath chemistry, but the rolls in the zinc pot are often the key: sink rolls, stabilizer rolls and correcting rolls work in the molten zinc, their surfaces continuously picking up dross, which is then pressed into the strip as it contacts the rolls.

Zinc-pot conditions are especially harsh: hot-dip galvanizing runs around 460℃, Galvalume around 600℃, where dross forms quickly and crystallizes hard, in floating, suspended and bottom forms — ordinary cleaning methods simply cannot cope.

Prescribe by defect: roll-surface dross — dedicated zinc-pot scraper on-line; roll instability — check the three-roll six-arm, bushings and bearing pads; floating/suspended dross — dross pump; zinc ash — nose extraction unit. The zinc pot is an integrated system; no single measure solves every problem.

Good News: Cooperation with Major Steel Group
Strip Defects? Roll Contamination Is the Culprit